MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Elexar® EL 3954-80 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Elexar® EL-3954-80 is a high performance thermoplastic elastomer designed for the electrical/wire & cable market. Elexar® EL-3954-80 is a lubricated, medium hardness grade suitable for both injection molding and extrusion.

Features: Filled; Halogen Free; High Density; High Specific Gravity; Lubricated; Medium Flow; Slip

Uses: Connectors; Grommets; Strain Reliefs; Wire & Cable Applications

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 200 °C
13 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  76
@Time 5.00 sec
76
@Time 0.00139 hour
ASTM D2240
 78
@Time 1.00 sec
78
@Time 0.000278 hour
ASTM D2240
Tensile Strength at Break 8.89 MPa1290 psiFlow; Die C, 20 in/min; ASTM D412
 11.7 MPa1700 psiAcross Flow; Die C, 20 in/min; ASTM D412
 13.1 MPa1900 psiExtruded Tape, Flow; Die C, 20 in/min; ASTM D412
Tensile Stress at Strain  2.83 MPa
@Strain 100 %
410 psi
@Strain 100 %
Across Flow; Die C, 20 in/min; ASTM D412
 3.92 MPa
@Strain 300 %
568 psi
@Strain 300 %
Across Flow; Die C, 20 in/min; ASTM D412
 3.94 MPa
@Strain 100 %
571 psi
@Strain 100 %
Flow; Die C, 20 in/min; ASTM D412
 4.70 MPa
@Strain 300 %
682 psi
@Strain 300 %
Flow; Die C, 20 in/min; ASTM D412
Elongation at Break 600 %600 %Extruded Tape, Flow; Die C, 20 in/min; ASTM D412
 640 %640 %Flow; Die C, 20 in/min; ASTM D412
 740 %740 %Across Flow; Die C, 20 in/min; ASTM D412
Tear Strength 38.0 kN/m217 pliFlow; Die C, 20 in/min; ASTM D624
 40.3 kN/m230 pliAcross Flow; Die C, 20 in/min; ASTM D624
Compression Set  29 %
@Temperature 22.8 °C,
Time 79200 sec
29 %
@Temperature 73.0 °F,
Time 22.0 hour
Type I; ASTM D395B
 63 %
@Temperature 70.0 °C,
Time 79200 sec
63 %
@Temperature 158 °F,
Time 22.0 hour
Type I; ASTM D395B
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 43.3 kV/mm1100 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746
UL RTI, Electrical 90.0 °C194 °FUL 746
UL RTI, Mechanical with Impact 50.0 °C122 °FUL 746
Flammability, UL94 HBHB0.06 in, All Colors
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 188 - 216 °C370 - 420 °F
Middle Barrel Temperature 188 - 216 °C370 - 420 °F
Front Barrel Temperature 188 - 216 °C370 - 420 °F
Nozzle Temperature 188 - 216 °C370 - 420 °F
Zone 1 177 - 204 °C350 - 400 °F
Zone 2 177 - 204 °C350 - 400 °F
Zone 3 177 - 204 °C350 - 400 °F
Zone 4 177 - 204 °C350 - 400 °F
Zone 5 177 - 204 °C350 - 400 °F
Die Temperature 177 - 204 °C350 - 400 °F
Melt Temperature 188 - 216 °C370 - 420 °FProcessing Temp
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNO780 / 128961

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.