MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Copper-Nickel-Phosphorus alloy, UNS C19000
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: springs, clips, electrical connectors, power tube and electron tube components, high-strength electrical components, bolts, nails, screws, cotter pins, and parts requiring some combination of high-strength, high electrical or thermal conductivity, high resistance to fatigue and creep, and good workability.

Available as flat products, rod, wire.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.87 g/ccC19200
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 262 - 793 MPa
Tensile Strength, Yield 138 - 552 MPaDepending on temper
Elongation at Break 50 %in 50.8 mm.
Tensile Modulus 18000 ksi
Machinability 30 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000290 ohm-cm60% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.80 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0920 BTU/lb-°F
Thermal Conductivity 145 BTU-in/hr-ft²-°F
Melting Point 1900 - 1980 °F
Solidus 1900 °F
Liquidus 1980 °F
Annealing Point 900 - 1300 °F
 
Processing PropertiesOriginal ValueComments
Precipitation Temperature >= 850 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 98.7 %
Nickel, Ni 1.1 %
Phosphorus, P 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1020 Steel, cold rolled
Overview of materials for High Carbon Steel
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
Scandium, Sc
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)

MC19000b1 / 10924

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.