MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik P84®UHT 40G HCM Aromatic Polyimide, 40% Graphite Filled
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes:
  • Excellent thermal-oxidative stability (use up to 300 ° C)
  • High mechanical strength and dimensional stability even at very high temperatures
  • Good creep resistance under load even at high temperatures
  • Easy machinability with standard tools for metals
  • Excellent tribological properties, high wear resistance
  • Processing by direct forming
Application examples: bushings, seals, bearings components, guides, gear wheels, and valve parts in the automotive and aerospace industries and in industrial equipment
Industrial Sector: Automotive and Mobility, Aircraft and Aerospace, Industry and Engineering
Processing: Hot compression molding, Machining
Delivery form: Pellets, Granules, Powder
Resistance to: Heat (thermal stability), Fire / burn, Wear / abrasion, Oil / fuels
Electrical: Conductive
Additives: Lubricant
Applications: Displays, Electrical and Electronical, General purpose, IT and telecommunication
Processing: DF Direct forming
Special Characteristics: Halogen-free, PTFE-free, Amorphous, High heat resistant, Non-dripping, Self-extinguishing, Thermally conductive
Features: Creep resistance, Low coefficient of friction, Lightweight
Color: Natural color, Black
Additives: Inorganic fillers
Chemical Resistance: Acid resistance, Solvent resistance, Grease resistance, Oil resistance, Oxidation resistance, Radiation resistance, Fuel resistance, General chemical resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.400 g/ccEN ISO 60
Density 1.67 g/ccISO 1183
Water Absorption 0.100 %
@Time 86400 sec
ISO 62
 0.100 %
@Time 173000 sec
ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 84.0ISO 7619-1
Tensile Strength at Break 77.0 MPaISO 527
Tensile Strength 77.0 MPaISO 527
Elongation at Break 1.70 %ISO 527
Tensile Modulus 8580 MPaISO 527
Flexural Strength 123 MPaISO 178
Flexural Modulus 8020 MPaISO 178
Compressive Strength 161 MPaISO 604
Compressive Modulus 7940 MPaISO 604
Charpy Impact Unnotched 7.00 kJ/m²Type of failure: C; ISO 179/1eU
Charpy Impact, Notched 2.00 kJ/m²Type of failure: C; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 4.38 W/m-KLFA, solid state; ISO 22007-4
Deflection Temperature at 0.46 MPa (66 psi) 364 °CISO 75-1/-2
Glass Transition Temp, Tg 282 °CDMA, 3 point bending; ISO 6721-5
 
Descriptive Properties
ColorNatural Color, Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7822 / 324954

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.