MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LB110 PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: General Description: LB110 is a homopolymer blending resin, which can be characterized with its fine particle size, medium molecular weight . It is used in plastically for viscosity , air released and gloss control. The fine particle size makes it useful for producing thin applications.

Main Applications: Plastically, Automotive underbody coater, Fabric coating, Flooring, Slush molding , Dipping

CAS No: 9002-86-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D790
Bulk Density 0.520 - 0.660 g/cc0.0188 - 0.0238 lb/in³ASTM D1895
Volatiles <= 0.40 %
@Temperature 110 °C,
Time 3600 sec
<= 0.40 %
@Temperature 230 °F,
Time 1.00 hour
ASTM D3030-90
Molecular Weight 60000 - 150000 g/mol60000 - 150000 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 302 °C576 °F
Ignition Temperature 435 °C815 °FAutoignition
 
Descriptive Properties
Degree of Polymerization900-100030°C, JIS K 6720-2
K-Value64DIN53726 / ISO1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® 58070 Thermoplastic Polyurethane
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer
LG Chemical SEETEC H5300 Polypropylene, Homopolymer
Kuraray Genestar™ GX1500A-M41 Nylon, 50% Glass Filled

PLAY723 / 148733

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.