MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC CYCOLOY™ FR Resin CX7720 Polycarbonate + ABS (PC+ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY CX7720 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable, high flow, high heat resistant, non chlorinated/brominated flame retardant grade. It has a UL94 V0@1.2mm, 5VA@2.5mm and 5VB@1.5mm flame rating. This grade has improved chemical resistance compared to standard PC/ABS blends and is a good candidate for thin wall applications.

Features: Hydrolytic Stability,Chemical Resistance,Flame Retardant,Thin Wall,Heat Stabilized,Good Mold Release

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Density 1.22 g/cc0.0441 lb/in³ISO 1183
Moisture Absorption 0.0400 %0.0400 %Injection Molding
 0.0700 %0.0700 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.15 %0.15 %ISO 62-1
Viscosity 22 cP
@Load 5.00 kg,
Temperature 260 °C
22 cP
@Load 11.0 lb,
Temperature 500 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  9.0 g/10 min
@Load 2.16 kg,
Temperature 260 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
 25 g/10 min
@Load 5.00 kg,
Temperature 260 °C
25 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psi50 mm/min; ISO 527
 66.0 MPa9570 psi50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa9430 psi50 mm/min; ASTM D638
 65.0 MPa9430 psi50 mm/min; ISO 527
Elongation at Break 122 %122 %50 mm/min; ISO 527
 126 %126 %50 mm/min; ASTM D638
Elongation at Yield 5.0 %5.0 %50 mm/min; ASTM D638
 5.0 %5.0 %50 mm/min; ISO 527
Tensile Modulus 2.86 GPa415 ksi50 mm/min; ASTM D638
 2.90 GPa421 ksi1 mm/min; ISO 527
Flexural Strength 97.0 MPa14100 psiyield, 2 mm/min; ISO 178
 99.0 MPa14400 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.09 GPa303 ksi2 mm/min; ISO 178
 2.81 GPa408 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 150 J111 ft-lbASTM D256
 63.0 J
@Temperature -30.0 °C
46.5 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²80*10*4; ISO 180/1A
 11.0 kJ/m²5.23 ft-lb/in²80*10*3; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 1.10 J/cm²5.23 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 62.0 J45.7 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=0.750 mm
15 - 30 sec
@Thickness >=0.0295 in
UL 746A
 30 - 60 sec
@Thickness >=1.50 mm
30 - 60 sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=0.750 mm
>= 120 arcs
@Thickness >=0.0295 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  60.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 60.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  65.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 65.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.6 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)  122 °C
@Thickness 3.20 mm
252 °F
@Thickness 0.126 in
unannealed; ASTM D648
 124 °C
@Thickness 6.40 mm
255 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 110 °C
@Thickness 3.20 mm
230 °F
@Thickness 0.126 in
unannealed; ASTM D648
 115 °C
@Thickness 6.40 mm
239 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 127 °C261 °FRate B/50; ISO 306
 127 °C261 °FRate B/50; ASTM D1525
 129 °C264 °FRate B/120; ISO 306
UL RTI, Electrical 100 °C212 °FUL 746B
UL RTI, Mechanical with Impact 100 °C212 °FUL 746B
UL RTI, Mechanical without Impact 100 °C212 °FUL 746B
Flammability, UL94  V-1
@Thickness >=1.00 mm
V-1
@Thickness >=0.0394 in
UL 94
 V-0
@Thickness >=1.20 mm
V-0
@Thickness >=0.0472 in
UL 94
 5VB
@Thickness >=1.50 mm
5VB
@Thickness >=0.0591 in
UL 94
 5VA
@Thickness >=2.50 mm
5VA
@Thickness >=0.0984 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 265 - 300 °C509 - 572 °F
Zone 2 260 - 300 °C500 - 572 °F
Zone 3 265 - 300 °C509 - 572 °F
Melt Temperature 270 - 300 °C518 - 572 °FInjection Molding
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 90.0 - 100 °C194 - 212 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00380 - 0.00760 cm0.00150 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80038 / 287985

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.