MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman CP814-01 Linear, Low-Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Rotational Molded

Material Notes: Description

CP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact.
Application

CP814-01 meets the specifications contained in FDA Regulation CFR 177.1520(c)3.1.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.924 g/ccASTM D792
ESCR 100% Igepal® 50 hourCondition C; ASTM D1692
Melt Index of Compound 50 g/10 minCondition E; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50ASTM D2240
Tensile Strength, Yield 1600 psi2"/min; ASTM D638
Elongation at Break 175 %2"/min; ASTM D638
Flexural Modulus, 1% Secant 46000 psiASTM D790
Falling Dart Impact 20.0 ft-lb
@Temperature -40.0 °C
ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -71.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 122 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) EX7C HF4750K High Density Polyethylene
Aaron Industries AAROLENE® ARPE HD 300-2 High Density Polyethylene Compounded Resin
Bamberger Polymers Bapolene® 3295 Polyethylene, Injection Grade
Dow DOWLEX™ IP-51 High Density Polyethylene Resin (HDPE)
Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite

PASHU073 / 25037

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.