52505UV is a HDPE copolymer which is manufactured in gas phase process. This grade is an injection molding grade for applications requiring a good physical property even at low temperatures, like pails, containers and technical moldings. Application: Containers. Features: Good physical property even at low temperatures. Additives: HD-52505: Thermal Antioxidant • HD-52505UV: Thermal Antioxidant UV Stabilizer.Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co. |