MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Samyang Triloy® 410N PC/PET alloy, Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Characteristics:
  • Impact resistant
  • Heat resistant
  • Dimensional stability
  • Processability
  • Flame retardant

Applications:

  • O/A part
  • Rear view mirror housing
  • Rice cooker base

All information provided by Samyang

Key Words: PC, PET
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0070 - 0.012 cm/cm
@Thickness 3.00 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115ASTM D785
Tensile Strength, Yield 550 kg(f)/cm²ASTM D638
Elongation at Break 80 %ASTM D638
Flexural Yield Strength 830 kg(f)/cm²ASTM D790
Flexural Modulus 23000 kg(f)/cm²ASTM D790
Izod Impact, Unnotched 60.0 kg-cm/cm
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+16 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 23.0 kV/mmASTM D149
Dissipation Factor 0.0090
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 121 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 83.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 105 °CASTM D648
Flammability, UL94 V-0
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 230 - 250 °C
Middle Barrel Temperature 220 - 240 °C
Front Barrel Temperature 210 - 230 °C
Nozzle Temperature 240 - 250 °C
Melt Temperature 240 - 250 °C
Drying Temperature 120 °C
Dry Time 3 - 5 hour
Moisture Content <= 0.020 %
Screw Speed 30 - 80 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Samyang Triloy® 450N Polymer Alloy, Blow Molding
Kingfa LONOY 2200 HT PC/PET Alloy
Kingfa LONOY 2100 LT PC/PET Alloy
Cheng Yu Plastic E500 PC/PET

PSAMY037 / 88119

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.