MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Oxygen-free Copper (OF), UNS C10200, H80 (16%) Temper, rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Wrought Copper

Material Notes: Test specimen: rod, 50mm diam.

Applications: busbars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass-to-metal seals, coaxial cables, klystrons, microwave tubes, and rectifiers.

Processing: Excellent hot and cold workability; good forgeability. Fabricated by bending, coining, coppersmithing, drawing and upsetting, hot forging and pressing, knurling, roll threading, shearing, spinning, swaging, and stamping.

Corrosion Resistance: Good to excellent. Susceptible to galvanic corrosion when coupled with iron, aluminum, magnesium, lead, tin, and zinc. Good resistance to atmospheric, brackish water, sea water, and non-oxidizing acid corrosion, but avoid heating in oxidizing atmospheres or exposing to oxidizing acids, moist halogens, sulfides, ammonia, or solutions with ammonium ions.

UNS C10200 - ASTM B12, B49, B124,B133, B187; C103 (UK); CDA 102 OF; CEN CW009A; Cu/cl NF A53301 (France); ISO Cu-OF R1337; JIS C1020 H3140 - bar (Japan); QQ-C-502

Key Words: ASTM B12, B49, B124, B133, B187, Cu/cl NF A53301 (France), BS C110, ISO Cu-OF R1337, CEN CW009A, oxygen free high conductivity copper (OFHC), C1020 H3140 - bar, QQ-C-502 rod, CDA 102 OF
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.94 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 45
Hardness, Rockwell F 85
Tensile Strength, Ultimate 310 MPa
 10.0 MPa
@Temperature 700 °C
 15.0 MPa
@Temperature 800 °C
 35.0 MPa
@Temperature 600 °C
 60.0 MPa
@Temperature 500 °C
 150 MPa
@Temperature 400 °C
 260 MPa
@Temperature 300 °C
 340 MPa
@Temperature 200 °C
 350 MPa
@Temperature 0.000 °C
bar
 360 MPa
@Temperature -50.0 °C
bar
 375 MPa
@Temperature -100 °C
bar
 390 MPa
@Temperature 100 °C
 420 MPa
@Temperature -150 °C
bar
 435 MPa
@Temperature 20.0 °C
 470 MPa
@Temperature -200 °C
bar
 530 MPa
@Temperature -250 °C
bar
Tensile Strength, Yield 275 MPa
@Strain 0.5 %
 1.00 MPa
@Strain 0.2 %,
Temperature 800 °C
 2.00 MPa
@Strain 0.2 %,
Temperature 700 °C
 10.0 MPa
@Strain 0.2 %,
Temperature 600 °C
 25.0 MPa
@Strain 0.2 %,
Temperature 500 °C
 125 MPa
@Strain 0.2 %,
Temperature 400 °C
 250 MPa
@Strain 0.2 %,
Temperature 300 °C
 325 MPa
@Strain 0.2 %,
Temperature 200 °C
 325 MPa
@Strain 0.2 %,
Temperature -50.0 °C
bar
 325 MPa
@Strain 0.2 %,
Temperature 0.000 °C
bar
 330 MPa
@Strain 0.2 %,
Temperature -100 °C
bar
 345 MPa
@Strain 0.2 %,
Temperature -150 °C
bar
 370 MPa
@Strain 0.2 %,
Temperature -200 °C
bar
 380 MPa
@Strain 0.2 %,
Temperature 100 °C
 390 MPa
@Strain 0.2 %,
Temperature -250 °C
bar
 420 MPa
@Strain 0.2 %,
Temperature 20.0 °C
Elongation at Break 20 %in 50 mm (2 in)
 17 %
@Temperature 200 °C
 17 %
@Temperature -50.0 °C
bar
 17 %
@Temperature 0.000 °C
bar
 19 %
@Temperature -100 °C
bar
 23 %
@Temperature 300 °C
 24 %
@Temperature 100 °C
 24 %
@Temperature -150 °C
bar
 27 %
@Temperature 20.0 °C
 31 %
@Temperature -200 °C
bar
 37 %
@Temperature 400 °C
 42 %
@Temperature -250 °C
bar
 46 %
@Temperature 500 °C
 48 %
@Temperature 600 °C
 53 %
@Temperature 700 °C
 60 %
@Temperature 800 °C
Reduction of Area 35 %
@Temperature 300 °C
 38 %
@Temperature 200 °C
 57 %
@Temperature 400 °C
 67 %
@Temperature 100 °C
 73 %
@Temperature 500 °C
 80 %
@Temperature 20.0 °C
 82 %
@Temperature 600 °C
 90 %
@Temperature 700 °C
 95 %
@Temperature 800 °C
Rupture Strength 5.20 MPa
@Temperature 650 °C,
Time 360000 sec
 9.70 MPa
@Temperature 650 °C,
Time 36000 sec
 17.0 MPa
@Temperature 450 °C,
Time 360000 sec
 33.0 MPa
@Temperature 450 °C,
Time 36000 sec
Modulus of Elasticity 115 GPa
Poissons Ratio 0.31
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %UNS C37700 (forging brass) = 100%
Shear Modulus 44.0 GPa
Shear Strength 180 MPa
Charpy Impact 118 J
@Temperature -250 °C
bar; V-notch
 132 J
@Temperature -200 °C
bar; V-notch
 135 J
@Temperature 0.000 °C
bar; V-notch
 138 J
@Temperature -150 °C
bar; V-notch
 139 J
@Temperature -50.0 °C
bar; V-notch
 140 J
@Temperature -100 °C
bar; V-notch
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000171 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 100 °C
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.385 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 391 W/m-K
@Temperature 20.0 °C
Melting Point 1083 °C
Annealing Point >= 700 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 375 - 650 °C
Hot-Working Temperature 750 - 875 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu >= 99.95 %includes silver (minimum 99.95% Cu+Ag)

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Oxygen-free Copper (OF), UNS C10200, H80 (35%), rod (25 mm Diameter)
Oxygen-free Copper (OF), UNS C10200, H80 (40%) rod, tubing (25 mm o.d. and 1.65 wall thickness)
Oxygen-free Copper (OF), UNS C10200, M20 temper, rod and shapes
Oxygen-free Copper (OF), UNS C10200, M20 temper, flat products

MC10200c3 / 10362

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.