MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

EMS-Grivory Grilamid® L 20 W 20 grey 9280 PA12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product Description: Grilamid L 20 W 20 grey 9280 is a semiflexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 grey 9280 is heat stabilized. The main features of Grilamid L 20 W 20 grey 9280 are:
  • Heat stability
  • Good impact strength
  • Good chemical resistance
  • Low weight, low density
  • Semi flexible
  • Low coefficient of friction
Application examples: Grilamid L 20 W 20 grey 9280 has been developed for small diameter tube extrusion applications in automotive and industrial market segments.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³Dry; ISO 1183
Water Absorption 1.5 %1.5 %Sim. to ISO 62
Moisture Absorption 0.700 %0.700 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 64
@Time 15.0 sec
64
@Time 0.00417 hour
Conditioned; ISO 868
Tensile Strength at Break 60.0 MPa8700 psiDry; ISO 527-1/-2
 60.0 MPa8700 psiConditioned; ISO 527-1/-2
Tensile Strength, Yield 30.0 MPa4350 psiDry; ISO 527-1/-2
 30.0 MPa4350 psiConditioned; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Nominal, Dry; ISO 527-1/-2
 >= 50 %>= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 20 %20 %Dry; ISO 527-1/-2
 20 %20 %Conditioned; ISO 527-1/-2
Tensile Modulus 0.500 GPa72.5 ksiConditioned; ISO 527-1/-2
 0.650 GPa94.3 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 32.0 kV/mm813 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 140 µm/m-°C77.8 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 160 µm/m-°C88.9 µin/in-°FISO 11359-1/-2
Melting Point 174 °C345 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C176 - 230 °FLong Term; ISO 2578
 150 °C302 °FShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AdditivesPlasticizer
AutomotivePowertrain and Chassis
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsMechanical Engineering
ProcessingOther Extrusion
Product AttributesFlexible
 Improved friction & wear properties

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRH035 / 156744

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.