MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik 29.8.2.L Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 29.8.2.L is a filler material suitable for welding the super duplex grade Sandvik SAF 2906. It is used for gas shielded arc welding and submerged arc welding. Sandvik 29.8.2.L is available as wire and rods.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 860 MPaSAW
 880 MPaTIG
Tensile Strength, Yield 660 MPa
@Strain 0.2 %
SAW
 670 MPa
@Strain 0.2 %
TIG
Elongation at Break 25 %TIG
 25 %SAW
Charpy Impact 115 JSAW
 150 JTIG
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.5 µm/m-°C
@Temperature 20.0 - 400 °C
Thermal Conductivity 16.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C >= 0.020 %SAW
 <= 0.025 %Filler Metal
 <= 0.025 %TIG
Chromium, Cr 28.5 %SAW
 29 %Filler Metal
 29 %TIG
Manganese, Mn 0.80 %SAW
 1.0 %Filler Metal
 1.0 %TIG
Molybdenum, Mo 2.3 %TIG
 2.3 %SAW
 2.4 %Filler Metal
Nickel, Ni 6.8 %TIG
 6.8 %SAW
 7.0 %Filler Metal
Nitrogen, N 0.32 %SAW
 0.35 %TIG
 0.36 %Filler Metal
Phosphorus, P <= 0.020 %Filler Metal
 <= 0.020 %TIG
 <= 0.020 %SAW
Silicon, Si 0.40 %Filler Metal
 0.40 %TIG
 0.60 %SAW
Sulfur, S <= 0.015 %Filler Metal
 <= 0.015 %TIG
 <= 0.015 %SAW

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5146 / 199710

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.