MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Glastic 4610-10-E Fiberglass-Reinforced Polyester Standoff Insulator
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: Glastic Standoff Insulators are molded of UL recognized flame resistant fiberglass-reinforced thermoset polyester molding compound. They feature shatter resistance and closer height tolerances than commonly available in porcelain insulators. Moisture and heat resistance properties of Glastic Insulators are higher than those of conventional insulators. UL recognized according to UL standard for safety 891.

Information provided by Glastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 138 MPa20000 psi
Crush Resistance 9070 kg20000 lb (mass)Compressive Strength
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 180 sec180 sec
Track Resistance 36000 sec36000 sec
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0
 
Descriptive Properties
Cantilever Strength in-lbs6000
Creep Distance in3-11/16
Dew Hi-Pot (volts) NEMA specs.15000
Dry Hi-Pot (volts) NEMA specs.19000
Height Tolerance in± 0.010
Impulse, volts600001.5x40 wave
Tensile Strength3000 lbs.
Torque Strength ft-lbs200

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling Glastic Laminates/Shapes TSF Fiberglass-Reinforced Polyester Laminate
Röchling Glastic Laminates/Shapes UTR Pultruded Tubing, Fiberglass-Reinforced Polyester
Röchling Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod
Röchling Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod
Röchling Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod

PGLASW1 / 41935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.