Description: Aegis PL165HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt viscosity and optimized crystallization properties, this formulation has been tailored to meet the demanding process behavior requirements of larger diameter extruded profiles. Chemical resistance is excellent to greases, oils and hydrocarbons. Applications:Used in extruded profile applications. Former Honeywell product; AdvanSix is a spin-off of Honeywell. |