System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Phillips Sumika Marlex® CDB-285 Polypropylene; Engineered Resin
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Molded
Material Notes:
Talc filled, scratch resistant, TPO for automotive interior applications.
Applications:
Information provided by Phillips
Phillips Sumika Polypropylene Company has been shut down, as announced in 2011.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.06
g/cc
ISO 1183
Linear Mold Shrinkage
0.0060
-
0.0080
cm/cm
48 hr at 23°C
0.0070
-
0.0090
cm/cm
48 hr at 80°C
0.0080
-
0.011
cm/cm
@Time 1800 sec
Melt Flow
26
g/10 min
@Temperature 230 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Hardness, Shore D
60
ISO 868
Tensile Strength, Yield
21.4
MPa
50 mm/min; ISO 527
Flexural Modulus
2.10
GPa
2.0 mm/min; ISO 178
Izod Impact, Notched (ISO)
3.00
kJ/m²
@Temperature -40.0 °C
ISO 180
21.0
kJ/m²
@Temperature 23.0 °C
ISO 180
Falling Dart Impact
28.0
J
6.6 m/s, Total Energy @ 0°C; ASTM D-3763
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
112
°C
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
60.0
°C
ISO 75
Processing Properties
Original Value
Comments
Rear Barrel Temperature
350
-
390
°F
Middle Barrel Temperature
410
-
455
°F
Front Barrel Temperature
410
-
455
°F
Nozzle Temperature
410
-
455
°F
Mold Temperature
73.0
-
120
°F
Back Pressure
50.0
-
150
psi
Descriptive Properties
Screw Speed %
30-60
Suggested Shot Size %
50-70
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Phillips Sumika Marlex® CHN-200 Thermoplastic Polyolefin
PCHEVD221 / 20715
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.