MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BIW Liquid Silicone Rubber, Self-Lubricating Grades
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Oil levels 2-5%. BIW produces molded parts with a range of adjustable properties from this two-component LSR system. No individual grade can fit all properties within the reported ranges.

Information provided by BIW Isolierstoffe GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 - 1.30 g/ccDIN 53479 A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30 - 70DIN 53505
Tensile Strength 5.00 - 10.0 MPaDIN 53504
Elongation at Break 400 - 900 %DIN 53504
Resilience 30 - 60Rebound; DIN 53512
Tear Strength 12.0 - 35.0 kN/mASTM D624 B
Compression Set 15 - 65 %
@Temperature 175 °C,
Time 79200 sec
DIN 53517
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+15 - 1.00e+16 ohm-cmVDE 0303
Dielectric Strength 20.0 - 30.0 kV/mmVDE 0303
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °CAll Colors
 280 °CBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials Silopren™ LSR 3286/40 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set
NuSil MED-4801 Liquid Silicone Rubber - Unrestricted Medical Use
Wacker Elastosil® LR 3065/30 A/B Liquid Silicone Rubber
Dow Silastic® 25784-V SILICONE RUBBER RED
Dow Silastic® 7-6840 BIOMEDICAL GRADE LSR, KIT

PBIWS981 / 192648

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.