MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik EUDRAGIT® FS 30 D Copolymer
Categories: Fluid

Material Notes: EUDRAGIT FS 30 D, the milky-white liquid of low viscosity with a faint characteristic odor is the aqueous dispersion of an anionic copolymer based on methyl acrylate, methyl methacrylate and methacrylic acid. It is insoluble in acidic media, but dissolves by salt formation above pH 7.0. Apart from its enteric properties, its dissolution at a higher pH value allows targeted colon delivery. With a glass transition temperature of 48°C, EUDRAGIT FS 30 D is a very flexible polymer. Due to the low minimum film forming temperature only small amounts of plasticizer are required to get a smooth film formation.

Physical properties: It is a milky-white liquid of low viscosity with a faint characteristic odor.

Characteristics:

  • A solubility above pH 7.0 allows specific colon targeting
  • Because of its flexibility it is particularly suitable for multi unit dosage forms
  • Matrix systems with EUDRAGIT FS 30 D will release 100% of the drug
  • Polymer amounts of 10 to 20 % are sufficient to get a pH-independent matrix
  • The flexibility of EUDRAGIT FS 30 D makes this polymer particularly suitable for the mixing with EUDRAGIT L 30 D-55
  • Amounts below 50 % do only influence the flexibility of the EUDRAGIT L 30 D-55 coating, not the release profile. With amounts > 75 % specific sites in the GI tract can be targeted.
CAS number: 26936 – 24 – 3

Chemical/ IUPAC name: Poly(methyl acrylate-co-methyl methacrylate-co-methacrylic acid) 7:3:1

INCI name: Acrylates Copolymer

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight 280000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 70[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 38.0 - 48.0 °C
 
Descriptive Properties
Minimum Film Forming Temp-14°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik EUDRAGIT® S 100 Copolymer
ASI® FS 30 Fast Setting Cyanoacrylate Instant Adhesive
Evonik EUDRAGIT® E PO Copolymer
Evonik EUDRAGIT® E 12, 5 Copolymer
S-Glass Fiber, Generic

PEVONIL826 / 197030

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.