MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Viton® GFLT-600S Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Cures exceptionally fast to a high state of cure
  • Similar to improved low temperature properties compared to Viton® GFLT
  • Improved mold release/mold fouling properties
  • Improved mold flow and less shear sensitivity for a 65 Mooney peroxy cured FKM
  • Excellent physical properties with high elongation, both original and aged
  • Heat, fluids, and low temperature resistance comparable to Viton® GFLT
  • Improved water resistance/lower volume swell in water
  • Excellent compression set resistance with either low or no postcure

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.86 g/ccUncompounded Viton
Mooney Viscosity 65
@Temperature 121 °C
ML (1+10), Uncompounded Viton; ASTM D1646
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68No Postcure; ASTM D1414
 702 hours Postcure; ASTM D1414
Tensile Strength at Break 12.2 MPaNo Postcure; ASTM D412
 15.9 MPa2 hours Postcure; ASTM D412
Tensile Stress at Strain 0.700 MPa
@Strain 10 %
No Postcure; ASTM D412
 0.700 MPa
@Strain 10 %
2 hours Postcure; ASTM D412
Elongation at Break 220 %2 hours Postcure; ASTM D412
 222 %No Postcure; ASTM D412
100% Modulus 0.00440 GPa
@Strain 100 %
No Postcure; ASTM D412
 0.00540 GPa
@Strain 100 %
2 hours Postcure; ASTM D412
Tear Strength 5.20 kN/m
@Temperature 150 °C
Compression Set 12 %
@Temperature 200 °C,
Time 79200 sec
O-Rings, postcured; ASTM D395B
 13 %
@Temperature 200 °C,
Time 79200 sec
O-Rings, no postcure; ASTM D395B
 18 %
@Temperature 200 °C,
Time 252000 sec
O-Rings, postcured; ASTM D395B
 21 %
@Temperature 200 °C,
Time 252000 sec
O-Rings no postcure; ASTM D395B
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -24.5 °CRetraction Temperature, Tr10
Glass Transition Temp, Tg -26.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 177 °C
@Time 299 sec
Cure
 232 °C
@Time 7200 sec
Postcure
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 67 %Uncompounded Viton
 
Descriptive Properties
Colorwhite to tanUncompounded Viton
Compound NumberA50-03
FormSheetUncompounded Viton
Formulation as Tested100GFLT-600S
 2Luperox® 101-XL45
 2Zinc Oxide
 3Diak 7 (TAIC)
 30MT Black
OdorNoneUncompounded Viton
Storage StabilityExcellentUncompounded Viton

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Viton® GF-600S Fluoroelastomer Compound
Chemours Viton® GBL-600S Fluoroelastomer Compound
Chemours Viton® GBL-200S Fluoroelastomer Compound
Chemours Viton® GBLT-600S Fluoroelastomer Compound
AISI 8740 Steel, annealed 815°C (1500°F)

PDVC9839 / 170480

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.