MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion ToughMet® 2 Strip 1/2 HT (TB00) Copper-Nickel-Tin Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: ToughMet 2 material is a high-performance, wrought, heat treatable, lead-free strip alloy that imparts superior mechanical performance and high thermal stability to plain bearing applications. The alloy has both excellent resistance to wear and high resistance to galling and seizing under high loads. In addition, the ToughMet 2 alloy’s high thermal conductivity provides effective heat dissipation in bearing applications. Parts are easily formed and can be machined either before or after heat treatment. ToughMet 2 heat treatment is a simple single- step process for three hours at 370 - 400°C (700 - 750°F). Heat treated ToughMet 2 bearings do not significantly work harden in service. ToughMet 2 strip is available in two tempers (A and ½ H) depending on the required strength and formability. ToughMet 2 alloy is compatible with conventional processing fluids, oils, and lubricants.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.91 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 290 - 350290 - 350
Tensile Strength 862 - 1030 MPa125000 - 150000 psi
Tensile Strength, Yield 689 - 827 MPa100000 - 120000 psi
Elongation at Break >= 6.00 %>= 6.00 %
Modulus of Elasticity 115 GPa16700 ksibefore heat treat
 140 GPa20300 ksiafter heat treat
Poissons Ratio 0.3000.300
Shear Modulus 44.0 GPa6380 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 200 °C
9.00 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.400 J/g-°C
@Temperature >=100 °C
0.0956 BTU/lb-°F
@Temperature >=212 °F
Thermal Conductivity 52.0 W/m-K361 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 85.0 %85.0 %
Nickel, Ni 9.00 %9.00 %
Tin, Sn 6.00 %6.00 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBBC113i / 323579

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.