MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
NuSil EPM-2493 Silicone, Thermal Interface Material (TIM): Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: General Purpose: Thermal Interface Material (TIM): Adhesives

Comments: Low viscosity for complex geometries

Cure system: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.34 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65
Tensile Strength at Break 1.20 MPa
Elongation at Break 50 %
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.00 W/m-K
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Temperature 150 °C
Working Life 13.0 hour
@Temperature 25.0 °C
 
Descriptive Properties
ColorWhite
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow
Aluminum, Al
Wacker Semicosil® 970 TC A/B Conductive Adhesive Sealant
Tra-Con Tra-Duct 2919 Room Temperature Conductive, Flexible Silver Epoxy Adhesive
Tra-Con Tra-Bond 813J01 Silicone Encapsulant

PNUSIL263 / 141987

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.