MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID® 66 GF 25 HTS 000/1M Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: PA66 for injection molding, reinforced with 25% glass fiber, heat stabilized, hydrolysis resistant. Stabilized against oil, hot oil, fats. Specially developed for bearing cages. Used and for cooling water systems in the automotive industry. Delivered in natural and black.

Information Provided by Plastcom spol. s r.o.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³STN EN ISO 1183-1
Linear Mold Shrinkage, Flow 0.0047 cm/cm0.0047 in/inSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0066 cm/cm0.0066 in/inSTN EN ISO 294-4
Melt Flow 3.0 g/10 min
@Load 0.325 kg,
Temperature 275 °C
3.0 g/10 min
@Load 0.716 lb,
Temperature 527 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 160 MPa23200 psiSTN EN ISO 527-2
Elongation at Break 3.0 %3.0 %STN EN ISO 527-2
Tensile Modulus 9.00 GPa1310 ksiSTN EN ISO 527-2
Flexural Strength 220 MPa31900 psiSTN EN ISO 178
Flexural Modulus 5.70 GPa827 ksiSTN EN ISO 178
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -20.0 °C
19.0 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 4.60 J/cm²
@Temperature 23.0 °C
21.9 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched  0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 0.700 J/cm²
@Temperature -20.0 °C
3.33 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmSTN 34 6460
Surface Resistance 1.00e+14 ohm1.00e+14 ohmSTN 34 6460
Dielectric Strength 40.0 kV/mm1020 kV/inSTN EN 60243-2
Comparative Tracking Index 400 V400 VA; STN EN 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDSC; STN EN ISO 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FSTN EN ISO 75-2 (A)
Vicat Softening Point 255 °C491 °FB; STN EN ISO 306
Flammability, UL94 HBHB
Glow Wire Flammability Index 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
STN EN 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
Moisture Content 0.15 %0.15 %STN EN ISO 3344
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPLACN927 / 282519

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.