MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makroblend® M525 PC+PET
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend

Material Notes: (PC+PBT) Blend, impact modified, easy release, injection molding grade. Makroblend M525 offers an exceptional low-temperature impact strength, good flowability and excellent chemical resistance. Manufactured according to GMP, tested only according to ISO 10993-5 and ISO 10993-10

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccISO 1183-1
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm1 hr; 90°C; b.o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0010 - 0.0020 cm/cm1 hr; 90°C; b.o. ISO 2577
Melt Flow 21 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 MPa50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 55.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %50 mm/min, Nominal; ISO 527-1,-2
Elongation at Yield 4.5 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2000 MPa1 mm/min; ISO 527-1,-2
Flexural Yield Strength 65.0 MPa
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 2000 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 45.0 kJ/m²
@Temperature -30.0 °C
ISO 180-A
 60.0 kJ/m²
@Temperature 23.0 °C
ISO 180-A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Comparative Tracking Index 100 VSolution B, M; IEC 60112
 225 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 100 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CISO 75-1,-2
Vicat Softening Point 122 °C
@Load 5.10 kg
120°C/h; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techno Polymer Techno ABS LM100 Transparent
Arkema Rilsan® Clear G170 Polyamide
Covestro Makroblend® AR205 PC+PET
Covestro Makrolon® 2458 Polycarbonate, Injection Grade
Envalior Novamid® 3010SR NAT PA66

PCOVEST0798 / 202581

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.