Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength. Main Characteristics: UV stabilizer, Medium viscosity and Ultra-clean Applications: Diffuser sheet/plate, Optical film and Appliances CAS: 103598-77-2 Information provided by LG Chemical |