MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes:

Information provided by Teknor Apex Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 - 0.940 g/ccASTM D792
Linear Mold Shrinkage 0.011 cm/cm24 hours; ASTM D955
 0.013 cm/cmAfter 30 min. at 180°F; ASTM D955
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 39 - 4510 second delay; ASTM D2240
Tensile Strength at Break 1100 psi20"/min Type 1; ASTM D412
Tensile Strength, Yield 1490 psiASTM D412
 1594.3 psi107% Retention, Air Oven Aged 42 days at 121°C
 1639 psi110% Retention, Air Oven Aged 42 days at 110°C
Elongation at Break 140 %
 181.5 %33% Retention, Air Oven Aged 42 days at 110°C
 203.5 %37% Retention, Air Oven Aged 42 days at 121°C
 550 %ASTM D412
Elongation at Yield 16 %ASTM D412
100% Modulus 1.22 ksi
@Strain 100 %
ASTM D412
300% Modulus 1.236 ksi
@Strain 300 %
ASTM D412
Flexural Modulus 42050 psiASTM D790
Izod Impact, Notched NBHeat Aging Performance 1000 hrs at 120°C
 NB
@Temperature -40.0 °C
Heat Aging Performance 1000 hrs at 120°C
Gardner Impact 300 in-lb
@Temperature -30.0 °C
Tensile Impact Strength >= 224 ft-lb/in²
Impact Test 200 in-lb
@Temperature -40.0 °C
At Yield. Deflection: 693 mils, Force: 425 lbs (Instrumented Impact, 9000 in/min)
 350 in-lb
@Temperature -40.0 °C
At Break. Deflection: 1359 mils, Failure Mode: Ductile (Instrumented Impact 9000 in/min)
Tear Strength 364 pliDie C; ASTM D1004
 
Thermal PropertiesOriginal ValueComments
CTE, linear 119 µm/m-°C
@Temperature -30.0 - 30.0 °C
CTE, linear, Transverse to Flow 117 µm/m-°C
@Temperature -30.0 - 30.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 62.5 °C
Deflection Temperature at 1.8 MPa (264 psi) 40.7 °C
Glass Transition Temp, Tg -55.9 °C
Flame Spread 30.2 in/minPass: Burn Rate- Max 100; FMVSS 302
 
Descriptive Properties
Fogging92, 3 hours at 100°C, Haake buchler

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer
Ductile Iron grade 60-40-18
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer
Teknor Apex Telcar® TL 2530A Thermoplastic Elastomer
Teknor Apex Sarlink® 3439DN Thermoplastic Elastomer

PTEKNO306 / 70049

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.