MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP8005 Black Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropylene, polyethylene, and TPO’s without special surface preparation. It can replace screws, rivets, plastic, welding, and two-step processes which include chemical etchants, priming or surface treatments in many applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 15000 - 30000 cPBase, DV-II, #7 sp, 20 rpm
 35000 - 55000 cPAccelerator, DV-II, #7 sp, 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
Tensile Modulus 58782 psiat 1% Strain
Shear Strength 50.0 psiOverlap, Toluene for 14 days, Cohesive Failure
 200 psiOverlap, PTFE, Adhesive Failure
 200 psiOverlap, Acetone for 14 days, Cohesive Failure
 400 psiOverlap, LDPE, Substrate Failure
 450 psiOverlap, Gasoline for 14 days, Cohesive Failure
 525 psiOverlap, Glass (3/16" thick), Substrate Failure
 575 psiOverlap, HIPS, Substrate Failure
 750 psiOverlap, UHMWPE, Substrate Failure
 750 psiOverlap, Polystyrene, Substrate Failure
 850 psiOverlap, HDPE/HDG, Adhesive/Cohesive Failure
 875 psiOverlap, PE, Substrate Failure
 925 psiOverlap, 71°C/100% RH salt water soak for 14 days, Cohesive Failure
 950 psiOverlap, 71°C/100% RH for 14 days, AF/CF
 950 psiOverlap, Diesel Fuel for 14 days, Substrate Failure
 975 psiOverlap, RT salt water soak for 14 days, Substrate Failure
 1000 psiOverlap, 71°C water soak for 14 days, Substrate Failure
 1000 psiOverlap, HCl for 14 days, Substrate Failure
 1000 psiOverlap, Isopropyl Alcohol for 14 days, Substrate Failure
 1025 psiOverlap, HDPE/Galvanealed, Substrate Failure
 1025 psiOverlap, HDPE/CRS, Adhesive/Cohesive Failure
 1025 psiOverlap, NaOH for 14 days, Substrate Failure
 1025 psiOverlap, Antifreeze Coolant for 14 days, Substrate Failure
 1075 psiOverlap, Plexiglas (PMMA), Substrate Failure
 1100 psiOverlap, HDPE, Substrate Failure
 1100 psiOverlap, Polycarbonate, Adhesive Failure
 1100 psiOverlap, 304 Stainless Steel (1/32" thick), Cohesive Failure
 1100 psiOverlap, Control, Substrate Failure
 1150 psiOverlap, PP, Substrate Failure
 1225 psiOverlap, Oily HDG, Adhesive/Cohesive Failure
 1425 psiOverlap, Gel Coat (3/16" thick), Substrate Failure
 1575 psiOverlap, ABS, Substrate Failure
 1900 psiOverlap, PVC, Substrate Failure
 2050 psiOverlap, Copper (1/16" thick), Cohesive Failure
 2075 psiOverlap, Aluminum (1/16" thick), Cohesive Failure
 2275 psiOverlap, CRS (1/32" thick), Adhesive Failure
 2500 psiOverlap, Green FRP, Cohesive Failure
 300 psi
@Temperature 82.0 °C
Overlap
 750 psi
@Temperature 82.0 °C
Overlap, HDPE, AF/CF
 900 psi
@Temperature -29.0 °C
Overlap, Green FRP, Adhesive Failure
 975 psi
@Temperature -29.0 °C
Overlap, HDPE, Adhesive Failure
 975 psi
@Temperature 82.0 °C
Overlap, Green FRP, AF/CF
 1025 psi
@Temperature 66.0 °C
Overlap, Green FRP, AF/CF
 1150 psi
@Temperature 66.0 °C
Overlap, HDPE, AF/CF
 1550 psi
@Temperature 49.0 °C
Overlap, Green FRP, AF/CF
 1875 psi
@Temperature 49.0 °C
Overlap, HDPE, AF/CF
 2400 psi
@Temperature 24.0 °C
Overlap
 2450 psi
@Temperature 23.0 °C
Overlap, Green FRP, Adhesive Failure
 2475 psi
@Temperature 23.0 °C
Overlap, HDPE, Adhesive Failure
Peel Strength 9.00 pliT-Peel, HDPE, Cohesive but shocky
 10.0 pliT-Peel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 125 µm/m-°CBelow Tg
 170 µm/m-°CAbove Tg
Glass Transition Temp, Tg 33.0 °Conset
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 hourTime to Handling Strength
 
Descriptive Properties
AppearanceBlackBase
 Black
 WhiteAccelerator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ArcelorMittal Dual Phase 780 LCE Y450 Very High Strength Cold Rolled Steel
ArcelorMittal Dual Phase 600 Very High Strength Hot Rolled Steel
ArcelorMittal Dual Phase 600 Very High Strength Cold Rolled Steel
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
ArcelorMittal Dual Phase 780 Very High Strength Hot Rolled Steel

PMM34669 / 169416

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.