MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Techmer ES HiFill® PA6/6 GB15 15% Glass Bead Filler
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Bead Filled

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Bead, 15% Filler by Weight

Additive: Lubricant

Features: Lubricated

Information provided by TP Composites, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
Water Absorption 0.90 %
@Time 86400 sec
0.90 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.017 cm/cm
@Thickness 3.17 mm
0.017 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
Tensile Strength, Yield 75.8 MPa11000 psiASTM D638
Elongation at Break 3.5 %3.5 %ASTM D638
Flexural Strength 117 MPa17000 psiASTM D790
Flexural Modulus 2.76 GPa400 ksiASTM D790
Izod Impact, Notched 0.320 J/cm
@Thickness 3.17 mm
0.600 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 2.03 J/cm
@Thickness 3.17 mm
3.80 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Strength 16.1 kV/mm410 kV/inMethod A (Short-Time); ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 59.4 µm/m-°C33.0 µin/in-°FASTM D696
Melting Point 255 °C491 °F
Deflection Temperature at 0.46 MPa (66 psi) 232 °C450 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FUnannealed; ASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® PA6 GB15 L BK 15% Glass Bead Filled
Techmer ES HiFill® ABS GB15 15% Glass Bead Filler
RTP Company RTP 102 GB 15  Polypropylene (PP) Glass Fiber 15% - Glass Bead 15 %
RTP Company RTP 100 MG 15 GB 15  Polypropylene (PP) Milled Glass 15% - Glass Bead 15%
Ravago Manufacturing Americas Hylon N2030GBHL Nylon 6, 30% Glass Beads, DAM

PTPC0317 / 136255

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.