MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dynasol Solprene® 1430 Styrene-Butadiene Rubber SBR Diblock Copolymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Solprene 1430 is a high molecular weight linear random -block styrene/butadiene copolymer with 40% styrene content, 30% present as a polystyrene block. A choice of either BHT free or phosphite free non-staining antioxidant systems is available, all FDA approved for use in food contact applications. It is a high purity polymer, essentially gel free with a very clear color. S-1430 is used as elastomeric impact modifier for plastics, especially in high gloss HIPS by the “in situ” polymerization process. It is also used in vulcanized shoe soles giving high hardness, flexibility and abrasion resistance with good processability. It is available in bales wrapped in rubber modified polystyrene film soluble in styrene monomer.

Applications:

  • Plastic modification

Information provided by Dynasol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccDIN-53479
Volatiles <= 0.75 %ASTM D-5668
Viscosity Measure 42.5 cStStyrene solution viscosity 5%; NM 300-32
Ash <= 0.20 %ASTM D-1416
 
Chemical PropertiesOriginal ValueComments
Styrene Content 31 %Block styrene; NM 202-07
 40 %ASTM D-5775
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Color Alpha, max10
Styrene insolubles<0.03%NM 300-15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dynasol Calprene® 1015 Styrene-Butadiene Rubber SBR Diblock Copolymer
Armacell Monarch® F-05013 (Black) Neoprene, EPDM, SBR Blend Foam
Dynasol Solprene® 1205 Styrene-Butadiene Rubber SBR Diblock Copolymer
Dow Buna® SB 1721 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
ATG s.r.l. SBR Styrene-Butadiene Rubber

PDYNA58 / 34804

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.