Characteristics:- Medium molecular weight
- Narrow molecular weight distribution
- Designed for high speed orientation
Applications: - Monofilament
- Slit tape
- Woven and knitted fabrics
- Specialty films
This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture. |