MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PolyPLASTY PolyTAN 44/65 Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: PolyTAN is a polyurethane elastomer with exceptional flexibility, abrasion resistance, and tear strength even at high loads.

  • abrasion resistance
  • high mechanical resistance
  • keeps its shape even after multiple mechanical loads
  • various hardness modifications
  • chemical resistance
  • good machinability
  • possibility of metal casting or casting engineering plastics (bandages, sprockets)
  • operating temperatures from –30°C to 80°C, for short periods up to 120 °C (up to 4 hours)
Very good strength, resistant to mineral oils and gasoline, high abrasion resistance, and very good damping properties. Uses:
  • sealing
  • packing
  • cuffs
  • machine pads
  • flexible coupling
  • dampening stops
  • cylinder coverings
  • pressure rollers
  • covers of casters for high loads and slow speeds
  • lining hoppers in construction and metallurgy
  • lining mixers of concrete and mortar mixtures
  • spatulas and lining moulds in the construction industry
  • wiper blades for snow ploughs
  • circulating belts for shunting and combing machines etc.
The material is destroyed at a temperature above +160 °C.

Information provided by PolyPLASTY.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccDIN 53479
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60 - 70
Tensile Strength >= 30.0 MPaDIN 53504
Elongation at Break 540 - 660 %DIN 53504
Rebound 45 %DIN 53512
Abrasion 50mm3; DIN 53516
Compression Set 50 %
@Temperature 70.0 °C,
Time 86400 sec
DIN 53517
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °CContinuous
 120 °C
@Time 14400 sec
Short Term
Minimum Service Temperature, Air -30.0 °C
 
Descriptive Properties
Colorred

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PolyPLASTY PolyTAN 15/65 Polyurethane
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
NEU NEUSoft™ 597-60A Industrial Ether TPU / SBC blend
Multibase TPSiV® 3340-60A Thermoplastic Silicone Vulcanizate

PPOLYPL905 / 197615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.