MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow Dowlex™ 2689G HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Product Description: Dowlex™ 2689G Polyethylene Resin is an ethylene-octene copolymer produced via INSITE™ Technology from Dow.
Main Characteristics: HDPE with excellent stiffness and processability
Complies with: (EU) No 10/2011; US FDA 21 CFR 177.1520© 3.1a
Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©3.1a; EU 10/2011

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.957 g/ccASTM D792
Melt Flow 0.85 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 3880 psiASTM D882
Film Tensile Strength at Yield, TD 3860 psiASTM D882
Film Elongation at Break, MD 560 %ASTM D882
Film Elongation at Break, TD 320 %ASTM D882
2% Secant Modulus 118000 psiMD; ASTM D882
 138000 psiTD; ASTM D882
Elmendorf Tear Strength MD 16 gMethod B; ASTM D1922
Elmendorf Tear Strength TD 350 gMethod B; ASTM D1922
Dart Drop Test 66.0 gASTM D1709A
Film Tensile Strength at Break, MD 4600 psiASTM D882
Film Tensile Strength at Break, TD 2150 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 271 °F
 
Optical PropertiesOriginal ValueComments
Haze 48 %ASTM D1003
Gloss 12 %
@Thickness 0.0508 mm
45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 433 °F
Blow-up Ratio (BUR) 2.5
 
Descriptive Properties
Film Puncture Resistance49 ft-lb/in3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF421 / 311114

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.