MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Label-Lyte® 90 LP Coated, High Sheen, Metallized, White Opaque OPP for Water-based Patch Label Applications  (discontinued **)
Categories: Polymer; Adhesive; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Coated, white, metallized polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement. This film is compatible with offset litho and UV-cured inks. It is designed to be used as a monoweb and provides excellent converting performance, including printing, sheeting, guillotine cutting, and label transfer on magazine-fed labelers, such as Krones Topmatic labeling equipment.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 91.4 microns3.60 mil
Coating Weight >= 43.7 g/m²>= 27.3 lb/ream520
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 86 %86 %510
Film Elongation at Break, TD 25 %25 %510
Film Tensile Strength at Break, MD 42.13 MPa6111 psi510
Film Tensile Strength at Break, TD 80.441 MPa11667 psi510
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 3.0 %
@Temperature 135 °C
3.0 %
@Temperature 275 °F
438
Shrinkage, TD 3.0 %
@Temperature 135 °C
3.0 %
@Temperature 275 °F
438
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 18 %18 %417
 
Descriptive Properties
Gurley Stiffness, MD, mgf18
Gurley Stiffness, TD, mgf30
Yield, in2/lb15800

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Label-Lyte® 85 LP-200M Mirror Finish, Metallized, White Opaque OPP for Water-based Patch Label Applications
Toagosei America Aron Alpha® Industrial Krazy Glue™ 403TB Cyanoacrylate Adhesive
LG Chemical SEETEC BS500 LDPE
LG Chemical SEETEC BF500 LDPE
LG Chemical SEETEC BC500 LDPE

PEXB488 / 37793

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.