MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Technoprene® A60K6 Glass-Reinforced Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Standard Technoprene® 30% Glass-Reinforced Polypropylene

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccASTM D792
Water Absorption 0.020 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0050 cm/cmSO.F.TER Method
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ASTM D785
Tensile Strength 90.0 MPaASTM D638
Flexural Strength 135 MPaASTM D790
Flexural Modulus 6200 MPaASTM D790
Izod Impact, Notched 110 J/m
@Temperature -20.0 °C
ASTM D256/A
 130 J/m
@Temperature 23.0 °C
ASTM D256/A
Charpy Impact Unnotched 40.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+15 ohmASTM D257
Dielectric Constant 2.6ASTM D150
Comparative Tracking Index >= 650 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 - 60.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 150 °CASTM D648
Vicat Softening Point 138 °C50°C/h at 50 N; ASTM D1525
Flammability, UL94 HB
@Thickness 3.20 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese SO.F.TER Technoprene® AK6HI Glass-Reinforced Polypropylene
Celanese SO.F.TER Technoprene® A60K6F Glass-Reinforced Polypropylene
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber
RTP Company RTP 104 HB Polypropylene (PP), Glass Fiber - UL94 HB
Celanese SO.F.TER Technoprene® AK6D Glass-Reinforced Polypropylene

PSOFS812 / 162276

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.