MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ho Hsiang Ching HG-550 SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The HG series is classed as the SEBS (STYRENE-ETHYLENE/BUTYLENE-STYRENE) hydrogenated grade of materials. This series combines well with hard plastic materials and have the softness of the elastomers, therefore, it can serve both appearance and anti-scratch functions. When using this material, its functions can be altered by adding different formulations or additives based on product requirements, for instance, adding anti-mildew and antibacterial will make the product life longer. The HG series is used in anti-slip pads/mats, business-type handles and a variety of toothbrushes. For example, the modern toothbrushes are not only becoming more ergonomic in handle grip, but also promoting the comfort and design by TPE/TPS utilization. Thus, the entire toothbrush looks more "fashionable", in the meantime, the functionality of the toothbrush was breaking the traditional style by using. The TPE /TPS material can be bonded on the grip and back of the brush head, besides, it also can be embedded in and be the bristle. All of which makes cleaning efficient! Thus, the HG series is always to be the best material for toothbrush. Suitable for most of the thermoplastic processing methods, such as injection molding, extrusion molding and so on. This material complies with EU RoHS, REACH-SVHC regulations, the Nonyl Phenol Ethoxylates (NPEO), Polynuclear Aromatic Hydrocarbons (PAHs), PFOS / PFOA, Nonylphenol (6P) and other safety tests.

Color: Natural Color / Black Color / Customized Color

The optimum combination of materials: PP / PE / EVA

Processing Method: Injection, Extrusion

Storage conditions: At room temperature, avoid direct sunlight, keep away from fire and avoid humid environment.

Information provided by Ho Hsiang Ching Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Melt Flow 20 - 30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
20 - 30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555ASTM D2240
Tensile Strength 2.45 MPa356 psiASTM 412C
Elongation at Break 500 %500 %ASTM 412C
Tear Strength 17.7 kN/m101 pliASTM 624C
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 70.0 °C158 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 177 °C320 - 351 °F
Middle Barrel Temperature 166 - 182 °C331 - 360 °F
Front Barrel Temperature 177 - 191 °C351 - 376 °F
Nozzle Temperature 182 - 204 °C360 - 399 °F
Mold Temperature 16.0 - 66.0 °C60.8 - 151 °F
Injection Velocity 13.0 - 25.0 mm/sec0.512 - 0.984 in/sec
Injection Pressure 34.0 - 69.0 MPa4930 - 10000 psi
Hold Pressure 14.0 - 48.0 MPa2030 - 6960 psi
Back Pressure 0.340 - 0.690 MPa49.3 - 100 psi
Screw Speed 50 - 70 rpm50 - 70 rpm
 
Descriptive Properties
Cold resistance temperature-40°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHSIANG001 / 312477

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.