System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Petropol Tenopom® A3 HF CNZA010 PR330 MSP POM
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
;
Acetal Homopolymer, Unreinforced
Material Notes:
Polyacetal homopolymer with high viscosity in gray color, easy processing, suitable for injection parts where it needs to be easily completed.
Information provided by Petropol
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.42
g/cc
0.0513
lb/in³
ASTM D792
Linear Mold Shrinkage
0.018
-
0.026
cm/cm
0.018
-
0.026
in/in
ASTM D955
Melt Flow
21.2
-
28.1
g/10 min
@Load 2.16 kg,
Temperature 190 °C
21.2
-
28.1
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
92
92
ASTM D785
Tensile Strength
71.0
MPa
10300
psi
ASTM D638
Elongation at Break
27 %
27 %
ASTM D638
Flexural Modulus
3.00
GPa
435
ksi
ASTM D790
Izod Impact, Notched (ISO)
7.00
kJ/m²
3.33
ft-lb/in²
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+14
ohm-cm
1.00e+14
ohm-cm
ASTM D150
Dissipation Factor
0.0050
@Thickness 1.00 mm,
Frequency 1e+6 Hz
0.0050
@Thickness 0.0394 in,
Frequency 1e+6 Hz
ASTM D149
Thermal Properties
Metric
English
Comments
Melting Point
178
°C
352
°F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi)
165
°C
329
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
110
°C
230
°F
ASTM D648
Flammability, UL94
HB
HB
Processing Properties
Metric
English
Comments
Processing Temperature
210
-
220
°C
410
-
428
°F
Molding
Mold Temperature
50.0
-
90.0
°C
122
-
194
°F
Drying Temperature
80.0
°C
176
°F
Dry Time
3.00
hour
3.00
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PPETROPOL376 / 313284
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.