MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MBA Polymers PP 2123 Post-consumer recycled polypropylene copolymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Available in standard black.

Information provided by MBA Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccMBA Method
Melt Flow 5.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 20.0 MPa
@Temperature 23.0 °C
ISO 527-2/50
Flexural Modulus 1000 MPa
@Temperature 23.0 °C
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature -20.0 °C
ISO 180/1A
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 210 °CExtrusion Range
 200 °CRecommended Extrusion
 200 °CRecommended Injection Molding
 190 - 220 °CInjection Molding Range
Mold Temperature 40.0 °CRecommended
 30.0 - 60.0 °C
Drying Temperature 80.0 °C
@Time 3600 - 7200 sec
Moisture Content <= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MBA Polymers PP 2131 F20 Post-consumer recycled polypropylene copolymer with approximately 20% fillers
A. Schulman Lucent CPP-0307 Polypropylene, Mineral Filled, Impact Modified
Nye Lubricants 920 (HSC) Synthetic Oil
MTM Plastics Dipolen® PP Recycled PP
MBA Polymers PP 2182 Post-consumer recycled polypropylene copolymer

PMBAP993 / 161700

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.