Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Plastcom SLOVAMID 66 GF 25 Polyamide 66, 25% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Features

Chemically reinforced with 25% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. With the increasing content of FG also the toughness, tensile and flexural strength increase, the shrinkage decreases and the heat application increases up to 150°C. It achieves higher rates of tensile strength and modulus of elasticity also in conditioning state when compared with PA 6 GF. Application: hobby tools, covers of electrotools, electromotors, cooling screws of blowers, gear wheels, carrying parts in the automotive industry like brake cables. Delivered in natural and in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccSTN 64 0111
Linear Mold Shrinkage 0.0078 cm/cmSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0118 cm/cmSTN 64 0808
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
STN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 165 MPaSTN EN ISO 527-2
Elongation at Break 3.0 %STN EN ISO 527-2
Tensile Modulus 7800 MPaSTN EN ISO 527-2
Flexural Strength 210 MPaSTN EN ISO 178
Flexural Modulus 6500 MPaSTN EN ISO 178
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 55.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 10.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmSTN IEC 60093
Surface Resistance 1.00e+14 ohmSTN IEC 60093
Dielectric Strength 40.0 kV/mmSTN IEC 60243
Comparative Tracking Index 400 VSTN 34 6468
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 250 °CSTN EN ISO 75/A
Vicat Softening Point 250 °CB; STN EN ISO 306
Flammability, UL94 HB
Glow Wire Test 650 °CSTN IEC 60695-2-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.15 %STN EN ISO 960
Injection Pressure 70.0 - 120 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 66 GF 15 Polyamide 66, 15% Glass Fiber
Covestro Bayblend® KU 2-1480 Polycarbonate/ABS Blend
CENTROPLAST CENTROCARB GF Polycarbonate 30% glass fiber
Plastcom SLOVAMID 66 GF 15 HI PA66, 15% glass fibre
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin

PPLACO042 / 106920

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.