MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Resin Technology Group CT-988 Cationic UV Cure Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: CT 988 is an epoxy-based, paste-viscosity, cationic-curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resistant, low out-gassing polymer system capable of surviving exposure up to 150°C.

Applications:

Disk drive applications, wire tack, non-acrylic UV bonding.

Processing:

UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometers

Recommended Aurora UV light sources:

  • Aurora 455-S 5x5 High Intensity Flood
  • Aurora 461-S 1x6 High Intensity Beam
  • Aurora 100-S Spot Light Guide

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080Cured
Elongation at Break 4.0 %4.0 %Cured
Shear Strength 27.6 MPa4000 psiCured, tensile
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 15.7 kV/mm>= 400 kV/inCured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °FCured
Minimum Service Temperature, Air -50.0 °C-58.0 °FCured
Flash Point >= 93.3 °C>= 200 °FUncured
 
Descriptive Properties
ColorTranslucent
CompositionEpoxy
Moisture ResistanceExcellentCured
Peel Shear Strength2
ToxicityLow
ViscosityLight PasteAt 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP21FL Flexibilized and Toughened Low Viscosity Epoxy
Lord Adhesives 312 General Purpose, Low Viscosity Epoxy Adhesive

PRESINT651 / 65535

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.