MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Buna CB 728 T Rubber, TX
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Buna CB 728 T is a solution high cis polybutadiene polymer produced with an organometallic neodymium catalyst.

CAS No: 9003-17-2

Production Plant: Orange, Tx

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.75 %ASTM D5668
Viscosity 160 cPsolution, 5.43% in toluene; IC-5a
Mooney Viscosity 44[ME]; ASTM D1645
 
Optical PropertiesOriginal ValueComments
Yellow Index <= 405 %Bulk; IC-69
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
@Temperature <=35.0 °C
 
Descriptive Properties
Content<150 ppmStyrene insoluble wet gel, IC-67

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lanxess Buna CB 70 GPT Rubber
Lanxess Buna CB 728 T Rubber
Lanxess Buna CB 530 T Rubber
Lanxess Buna CB 22 Rubber, TX
Lanxess Buna CB 45 Rubber (Texas Plant)

PLANY8478 / 208871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.