MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

MOL Group TIPOLEN FC 243-51 LDPE, Film Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Description: TIPOLEN FC 243-51 is a film grade of low density polyethylene with good molten stability and excellent processability. The films made of this grade have good mechanical properties. The grade does not contain any additives.

Applications: TIPOLEN FC 243-51 is intended for general purpose films, bubble films and foamed sheets. Recommended film thickness is 0.02 to 0.1 mm.

(1) Density, Vicat Softening Temperature and Shore D Hardness have been measured on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291) (2) Properties on film in M.D./T.D. - thickness of 0.07 mm (MFR=0.3 g/10min) and 0.04 mm (MFR more than 0.3 g/10min), blow up ratio 2:1

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³1; ISO 1183-1
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 51511; ISO 868
Film Elongation at Break, MD 300 %300 %2; ISO 527-1,3
Film Elongation at Break, TD 600 %600 %2; ISO 527-1,3
Dart Drop Test 80.0 g0.176 lb2; ISO 7765-1 method A
Film Tensile Strength at Break, MD 24.0 MPa3480 psi2; ISO 527-1,2
Film Tensile Strength at Break, TD 19.0 MPa2760 psi2; ISO 527-1,3
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 94.0 °C201 °F1; ISO 306/A 50
 
Optical PropertiesMetricEnglishComments
Haze 10 %10 %2; ASTM D 1003
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 200 °C320 - 392 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOLG009 / 297175

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.