MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® R525J NT0721 Nylon 66, 25% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Vydyne R525J NT0721 is a natural, 25% glass-filled, high-flow PA66 that is heat-stabilized with an electrically neutral heat stabilizer. It is specially designed for electrical applications requiring high dielectric strength, low conductivity and corrosion resistance.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccDAM; ISO 1183
Water Absorption 0.90 %
@Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 2.0 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 117 MPa50% RH; ISO 527-2
 174 MPaDAM; ISO 527-2
Elongation at Break 3.0 %DAM; ISO 527-2
 7.0 %50% RH; ISO 527-2
Tensile Modulus 5500 MPa50% RH; ISO 527-2
 8600 MPaDAM; ISO 527-2
Flexural Strength 150 MPa50% RH; ISO 178
 250 MPaDAM; ISO 178
Flexural Modulus 5700 MPa50% RH; ISO 178
 7700 MPaDAM; ISO 178
Poissons Ratio 0.40ISO 527-2
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 10.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 15.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 55.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 65.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 66.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 67.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm
@Thickness 1.00 mm
DAM; IEC 60093
Dielectric Strength 24.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
Arc Resistance 120 - 180 sec
@Thickness 3.00 mm
PLC 5; ASTM D 495
Comparative Tracking Index 600 V
@Thickness 3.00 mm
IEC 60112
Hot Wire Ignition, HWI 7.0 - 15 secPLC 4; UL 746
 7.0 - 15 secPLC 4; UL 746
 7.0 - 15 secPLC 4; UL 746
High Amp Arc Ignition, HAI >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/minPLC 1; UL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 109 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 245 °CUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical 120 °C
@Thickness 0.750 mm
UL 746
 120 °C
@Thickness 1.50 mm
UL 746
 120 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 85.0 °C
@Thickness 0.750 mm
UL 746
 85.0 °C
@Thickness 1.50 mm
UL 746
 105 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 115 °C
@Thickness 0.750 mm
UL 746
 120 °C
@Thickness 1.50 mm
UL 746
 120 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 HB
@Thickness 0.750 mm
 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 310 °CInjection
Middle Barrel Temperature 280 - 310 °CInjection
Front Barrel Temperature 280 - 310 °CInjection
Nozzle Temperature 280 - 310 °CInjection
Melt Temperature 285 - 305 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
Agency RatingsASTM, D4066 PA012G25
 ASTM, D6779 PA012G25
AppearanceNatural Color
FeaturesChemical Resistant
 Corrosion Resistant
 Good Colorability
 Good Electrical Properties
 Good Mold Release
 High Flow
 High Strength
 Laser Markable
 Organic Heat Stabilized
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Conditioned)
Ascend Performance Materials Vydyne® R525J BK0722 Nylon 66, 25% Glass Filled
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry)

PASCE9793 / 220896

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.