MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Nappar™ 6 Naphthenic Fluid
Categories: Fluid

Material Notes: Appearance: Clear/Transparent Liquid

Availability: Africa & Middle East and Europe

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.33 lb/gal
@Temperature 15.0 °C
ISO 12185
Kinematic Viscosity 0.86 cStASTM D445
Vapor Pressure 80.0 torr
@Temperature 20.0 °C
ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Boiling Point 174 °FInitial; ASTM D1078
Flash Point <= 32.0 °FASTM D56
 
Descriptive Properties
Aniline Point99°FMethod E, ASTM D611
Aromatic Content1 wt ppmUV, ExxonMobil Method
Dry Point181°FASTM D1078

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Isopar™ L (AP) Isoparaffin Fluid
Lubriplate 68-N Naphthenic Refrigeration Compressor Oil
ExxonMobil Jayflex™ 210 Naphthenic Hydrocarbon Plasticizer
ExxonMobil Isopar™ N Isoparaffin Fluid
ExxonMobil Isopar™ M (EU) Isoparaffin Fluid

PEX99643 / 175879

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.