MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay MACKAM® 2C LVA Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Mackam 2C-LVA is a mild amphoteric foaming and cleansing agent that can reduce the overall irritation of cleansing products into which it is formulated. It is often used as a detoxifying agent in baby shampoos. This material is compatible with anionic, non-ionic and most cationic systems. Mackam 2C-LVA aids in flash foaming and improves the foam stability of most formulations. This particular grade exhibits a significantly lower viscosity than others, making it very easy to empty containers and pump.

Infrared Spectrum: Matches Standard

INCI NAME: Disodium Cocamphodiacetate

CAS: 68650-39-5

EINECS: 272-043-5

Uses: Shampoos and Hand Soaps, Bubble Bath, Body Wash, Remoistened Wipes, Hospital Cleansers and Hard Surface Cleaners.

Information provided by Rhodia, Rhodia has been acquired by Solvay. The Mackam® brand has been sold to Verdant Specialty Solutions, although this specific grade has been discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 46.6 - 54.5 %Karl Fisher
pH 8.0 - 8.5
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 5.0
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear Liquid
CompositionPropylene GlycolReport
 Sodium Chloride10.5-12.5%
 Solids,-(NaCl + Propylene Glycol)35.5-38%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay GEROPON® CYA/75 Surfactant
Solvay MACKANATE® OPV-N Surfactant
Solvay ANTAROX® L 61 Surfactant
Solvay ANTAROX® 17-R-4 Surfactant
Solvay ANTAROX® L 64 Surfactant

WRHOD194 / 137425

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.