MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chengdu Letain CE-2202 PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Resin of LTP CE-2200 serials is a kind of engineering plastic with high performance based on PPS. For its excellent electric conduction property, it is mainly applied in thermostatic parts or shell for electric heating instrument. Thermal conduction and insulation materials made by Resin of LTP CE-2200 serials have these characteristic: high temperature control precise, resistance to water, oil-proof, good safety, light weight and wear well.

Information provided by Chengdu Letain Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 - 1.90 g/cc0.0578 - 0.0686 lb/in³ASTM-D792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/in80×80×3
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 100 - 125 MPa14500 - 18100 psiGB/T1040
Elongation at Break 1.2 %1.2 %GB/T1040
Flexural Strength 120 - 150 MPa17400 - 21800 psiGB/T1042
Flexural Modulus 80.0 - 120 GPa11600 - 17400 ksiGB/T1042
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²GB/T1043
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+8 - 1.00e+10 ohm-cm1.00e+8 - 1.00e+10 ohm-cmGB/T1410
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature >= 260 °C>= 500 °FGB1634

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGLT030 / 255883

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.