MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVASTER® B1 GF 10 Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: PBT for injection molding, reinforced with 10% glass fiber. Melt is characterized by very good rheology, which enables manufacturing of multiple products with complicated flow.

Application in the automotive, electrical and engineering industry - connectors of cable harnesses, car-door locks, connection links, grips etc. Delivered in natural and in the full RAL color scale.

Information Provided by Plastcom spol. s r.o.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccSTN EN ISO 1183-1
Linear Mold Shrinkage, Flow 0.0099 cm/cmSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0133 cm/cmSTN EN ISO 294-4
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 250 °C
STN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 87.0 MPaSTN EN ISO 527-2
Elongation at Break 4.0 %STN EN ISO 527-2
Tensile Modulus 5250 MPaSTN EN ISO 527-2
Flexural Strength 130 MPaSTN EN ISO 178
Flexural Modulus 3800 MPaSTN EN ISO 178
Charpy Impact Unnotched 43.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 49.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 7.00 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmSTN 34 6460
Surface Resistance 1.00e+15 ohmSTN 34 6460
Dielectric Strength 28.0 kV/mmSTN EN 60243-2
Comparative Tracking Index 350 VA; STN EN 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 200 - 220 °CDSC; STN EN ISO 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 135 °CSTN EN ISO 75-2 (A)
Vicat Softening Point 203 °CB; STN EN ISO 306
Flammability, UL94 HB
Glow Wire Flammability Index 750 °C
@Thickness 3.00 mm
STN EN 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °C
Mold Temperature 50.0 - 80.0 °C
Drying Temperature 120 °C
@Time 14400 sec
Moisture Content 0.10 %STN EN ISO 3344
Injection Pressure 60.0 - 100 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPLACN942 / 282534

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.