MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon N-Methylpiperazine (NMP) 1-methylpiperazine
Categories: Other Engineering Material

Material Notes: N-Methylpiperazine (NMP) is another cyclic ethylene amine which appears as a clear, hygroscopic liquid. NMP is primarily used as raw material for pharmaceuticals.

CAS number: 109-01-3

EINECS/ELINCS No: 203-639-5

Molecular formula: C5H12N2

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³
pH 11 - 1211 - 125% solution
Molecular Weight 100.19 g/mol100.19 g/mol
Vapor Pressure 0.00678 bar5.09 torr
 
Thermal PropertiesMetricEnglishComments
Melting Point 5.57 °C
@Pressure 0.1013 MPa
42.0 °F
@Pressure 14.69 psi
Boiling Point 133.66 °C
@Pressure 0.1013 MPa
272.59 °F
@Pressure 14.69 psi
Flash Point 31.5 °C88.7 °F101300; ISO 3679
Ignition Temperature >= 100 °C>= 212 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.20 %<= 0.20 %MOA 305
 
Descriptive Properties
AppearanceClear liquid
Assay= 99.0 wt%MOA 506
Color= 20 HazenMOA 201
Content= 0.5 wt%Organic impurities (MOA 506)
OdorAmmonical
Partition coefficient-0.57N-octanol/water, 25°C, log Pow
Vapor Density3.4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY714 / 286237

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.