System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Reliance Industries Reclair F18010 Polyethylene
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Linear Low Density (LLDPE)
;
Linear Low Density Polyethylene (LLDPE), Injection Molded
Material Notes:
Butene comonomer based Linear Low Density Polyethylene blow film grade.
Applications:
lamination films.
Information provided by Reliance Industries
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.918
g/cc
0.0332
lb/in³
ASTM D1505
Melt Flow
0.90
g/10 min
@Load 2.16 kg
0.90
g/10 min
@Load 4.76 lb
ASTM D1238
Mechanical Properties
Metric
English
Comments
Film Tensile Strength at Yield, MD
12.5
MPa
1810
psi
ASTM D882
Film Tensile Strength at Yield, TD
12.0
MPa
1740
psi
ASTM D882
Film Elongation at Break, MD
650 %
650 %
ASTM D882
Film Elongation at Break, TD
800 %
800 %
ASTM D882
Elmendorf Tear Strength, MD
3.30
g/micron
83.8
g/mil
ASTM D1922
Elmendorf Tear Strength, TD
10.3
g/micron
262
g/mil
ASTM D1922
Dart Drop
3.50
g/micron
88.9
g/mil
F
50
,38mm dart 66mm height; ASTM D1709
Film Tensile Strength at Break, MD
38.0
MPa
5510
psi
ASTM D882
Film Tensile Strength at Break, TD
30.0
MPa
4350
psi
ASTM D882
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Reliance Industries Reclair O21010 Polyethylene
Reliance Industries Reclair O19010 Polyethylene
Reliance Industries Reclair F18020 Polyethylene
Reliance Industries Reclair F19010 Polyethylene
Reliance Industries Reclair F22020 Polyethylene
PREL084 / 65424
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.