Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties. Applications: - Shafts
- Knives
- Fasteners
- Surgical applications
- Domestic applications
Available in cold rolled narrow strip and rod forms. |
EN 1.4028; ASTM 420; JIS SUS 420J2 |