MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hippe EP GM 202 Glass Mat Reinforced Epoxy Resin - Sheet
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 - 1.90 g/ccIEC 1212-2 8.1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 250 MPaIEC 1212-2 5.7
Flexural Strength >= 320 MPaPerpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 15.0 GPaIEC 1212-2 5.2
Compressive Strength >= 350 MPaPerpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 20.0 MPaParallel to laminations; IEC 1212-2 5.6
Izod Impact, Unnotched (ISO) >= 54.0 kJ/m²Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched >= 50.0 kJ/m²Parallel to laminations; IEC 1212-2 5.5.2
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance >= 5.00e+9 ohmAfter immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 5.5
@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
 <= 5.5
@Frequency 1e+6 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 35000 V
@Temperature 90.0 °C
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor <= 0.050
@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
 <= 0.050
@Frequency 1e+6 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 200 VIEC 1212-2 6.4
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0IEC 1212-2 7.2
 
Descriptive Properties
Thermal Endurance130 T.I.IEC 1212-2 7.1
Water Absorption< 40 mgIEC 1212-2 8.2; Test piece 50 x 50 x 10 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric
Kuraray Genestar™ GX1500A-M41 Nylon, 50% Glass Filled
Hippe EP GM 201 Glass Mat Reinforced Epoxy Resin - Sheet

PHIPPE908 / 121912

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.