MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Clwyd Compounders FEPM C Tetrafluoroethylene- propylene copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Tetrafluoroethylene propylene (FEPM, TFE/P), also known as Aflas®,1, is a partially fluorinated polymer that is composed of both propylene and tetrafluoroethylene monomers which can be crosslinked using a variety of curatives such as peroxides

Typical applications: Tetrafluoroethylene propylene is widely used in the chemical, automotive, aerospace, and oil industry. It provides some of the best all-around chemical resistance, very low gas permeability and is mainly used for the manufacture of seals and wire and cable insulation operating in harsh environments. The typical service temperature of FEPM is between -10C and +230°C (+445°F). However, at high service temperatures FEPM is rather weak, so that the design must prevent any high loads.

Advantages: This type of a copolymer offers a combination of high temperature and chemical resistance. Similar to other fluoroelastomers, it has excellent resistance to a broad range of chemicals including acids, bases, ozone, oxidizers, corrosion inhibitors, (hydraulic) oils, phosphate esters, alcohols and hot water/steam.

Disadvantages: FEPM is not compatible with aromatic and chlorinated hydrocarbons, and some fairly common organic solvents such as MEK, toluene, acetic acid, and acetone. Some other major disadvantages include high compression set, high glass transition temperature, low cold temperature performance, and poor extrusion resistance, especially at high temperatures, which makes FEPM difficult to process. Furthermore, it is rather expensive and, thus, only used when the components have to withstand harsh environments.

Information provided by CLWYD COMPOUNDERS LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 60 - 9560 - 95
Tensile Strength <= 25.0 MPa<= 3630 psi
Elongation at Break <= 250 %<= 250 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 300 °C572 °FUpper continuous
Minimum Service Temperature, Air 0.000 °C32.0 °Fsealing applications
 0.000 °C32.0 °Fnon-brittle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCLWYD001 / 316018

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.