MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Viton® 10 Process Aid
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Description: Viton® FreeFlow™ 10 is a fluoroelastomer additive in pellet form. It can be added to high density polyethylene (HDPE), linear low density polyethylene (LLDPE), or polypropylene (PPE).

Advantages:

  • Process improvements in all types of polyolefins including HDPE, low density polyethylene (LDPE), LLDPE, and PPE
  • Elimination or minimization of surface imperfections (e.g., melt fracture)
  • Reduction of die pressure, power requirements, and temperature
  • Increased output (at constant die pressure and temperature)
  • Improved properties when narrow dies are used in place of wide dies to reduce orientation

Information provided by manufacturer.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.78 - 1.84 g/cc
 
Descriptive Properties
AppearanceSilver gray to pale amber free flowing pellets
Package Stability4 yr
Packaging25 kg box

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Viton® A-200 with Blanc Fixe Fluoroelastomer Compound
Chemours Viton® A-200 with Celite 350 Fluoroelastomer Compound
Chemours Viton® A-100 Fluoroelastomer Compound
Chemours Viton® 40 Process Aid
Chemours Viton® A-200 with 30 MT Black and 2.5 VC50 Fluoroelastomer Compound

PDVDA67 / 34036

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.