MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASI® MP532092O Optical Grade Acrylate Solvent UV-Curing Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: MP532092O is a high performance UV curing adhesive engineered to bond glass and plastics. It is a flexible dual cure adhesive. This product can be cured under UV light or heat. Our MP532092O is a leading performer when used for bonding optical applications and general industrial applications. MP532092O is often cured with an electroless lamp D, medium pressure metal halide lamp. This UV adhesive also works well with UV light emitted diodes (UV LED) at wavelengths of 365 nm to 395 nm. Heat can be carried out at 120°C for 30 minutes. Design engineers select MP532092O for the optimum in finished product quality, reliability, performance, and cost effectiveness. MP532092O is an essential tool in improving overall product quality, lowering per unit cost, and reducing processing time. Benefits: Superior Bond Strength, Solvent Free, Low Odor, Improves Finished Product Quality Durable, Good Impact and Vibration Resistance, Easily Automated, No Clean Up. Substrate Applications: Soft fillings for Glass and PMMA, Dam or sealant for Glass, Plastic.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³uncured
Water Absorption  2.4 %
@Temperature 25.0 °C,
Time 86400 sec
2.4 %
@Temperature 77.0 °F,
Time 24.0 hour
cured
 4.3 %
@Temperature 100 °C,
Time 7200 sec
4.3 %
@Temperature 212 °F,
Time 2.00 hour
cured
Viscosity 1800 - 2600 cP
@Temperature 25.0 °C
1800 - 2600 cP
@Temperature 77.0 °F
20 rpm. Uncured
Linear Mold Shrinkage 0.018 cm/cm0.018 in/incured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 1414
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant <= 4.0<= 4.0cured
Dielectric Strength >= 15.7 kV/mm>= 400 kV/incured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg 9.00 °C48.2 °Fcured
Flash Point 103 °C217 °Funcured
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.48771.4877cured
 
Descriptive Properties
Blue FluorescingNo. Cured
Chemical ClassAcrylate Solvent
Color / appearancecolorless liquid
Flexible at Room Temperature?Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm Plexiglas® XT Soundstop® Extruded Acrylic
Trinseo Plexiglas® V825 Acrylic
Röhm Plexiglas® XT Grey 99561 RP Extruded Acrylic Sheet
Röhm PLEXIGLAS® XT Clear 0A070 UV transmitting PMMA
Röhm Plexiglas® XT 0A070 (29070) Extruded Acrylic

PASINC9158 / 233524

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.